Tested the white pla pro one only a little doesnt feed great very picky for the mags. This one is pa6cf .6 nozzle 9 hour print. annealed for 14 hours will test soon.
Tested the white pla pro one only a little doesnt feed great very picky for the mags. This one is pa6cf .6 nozzle 9 hour print. annealed for 14 hours will test soon.
Where did you get the white mag from?
It’s unseenkillers TOR mag requires metal feed lips from riptide rails